Synthesis, phase transition and negative thermal expansion of cubic Zr(W1 − y Mo y )2 − x V x O8 − x /2 (y =0.10, 0.20, 0.30, 0.40; 0⩽ x ⩽0.40) solid solutions

Cubic Zr(W1− y Mo y )2− x V x O8− x /2 (y =0.10, 0.20, 0.30, 0.40; 0⩽ x ⩽0.40) with negative thermal expansion property successfully obtained through an ASH process have different solid solubilities 15mol%, 13mol%, 12mol% and 11mol%, respectively.

Gespeichert in:
Autor*in:

Chen, Xi [verfasserIn]

Guo, Fuli

Deng, Xuebin

Tao, Juzhou

Qiu, Danli

Zhao, Xinhua

Format:

E-Artikel

Sprache:

Englisch

Erschienen:

2014

Schlagwörter:

Solid solutions

Negative thermal expansion

Phase transition

Umfang:

7

Übergeordnetes Werk:

Enthalten in: Factors associated with canine resource guarding behaviour in the presence of people: A cross-sectional survey of dog owners - Jacobs, Jacquelyn A. ELSEVIER, 2017, JAL : an interdisciplinary journal of materials science and solid-state chemistry and physics, Lausanne

Übergeordnetes Werk:

volume:612 ; year:2014 ; day:5 ; month:11 ; pages:252-258 ; extent:7

Links:

Volltext

DOI / URN:

10.1016/j.jallcom.2014.05.187

Katalog-ID:

ELV012466824

Nicht das Richtige dabei?

Schreiben Sie uns!