Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals
Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the...
Ausführliche Beschreibung
Autor*in: |
Xie, Ying [verfasserIn] |
---|
Format: |
E-Artikel |
---|---|
Sprache: |
Englisch |
Erschienen: |
2018transfer abstract |
---|
Schlagwörter: |
---|
Umfang: |
6 |
---|
Übergeordnetes Werk: |
Enthalten in: Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations - Crowley, Martha ELSEVIER, 2018, an international journal on the physics and chemistry of optical materials and their applications, including devices, Amsterdam [u.a.] |
---|---|
Übergeordnetes Werk: |
volume:77 ; year:2018 ; pages:13-18 ; extent:6 |
Links: |
---|
DOI / URN: |
10.1016/j.optmat.2018.01.015 |
---|
Katalog-ID: |
ELV042142768 |
---|
LEADER | 01000caa a22002652 4500 | ||
---|---|---|---|
001 | ELV042142768 | ||
003 | DE-627 | ||
005 | 20230626000638.0 | ||
007 | cr uuu---uuuuu | ||
008 | 180726s2018 xx |||||o 00| ||eng c | ||
024 | 7 | |a 10.1016/j.optmat.2018.01.015 |2 doi | |
028 | 5 | 2 | |a GBV00000000000669.pica |
035 | |a (DE-627)ELV042142768 | ||
035 | |a (ELSEVIER)S0925-3467(18)30015-6 | ||
040 | |a DE-627 |b ger |c DE-627 |e rakwb | ||
041 | |a eng | ||
082 | 0 | 4 | |a 300 |q VZ |
084 | |a 70.00 |2 bkl | ||
084 | |a 71.00 |2 bkl | ||
100 | 1 | |a Xie, Ying |e verfasserin |4 aut | |
245 | 1 | 0 | |a Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals |
264 | 1 | |c 2018transfer abstract | |
300 | |a 6 | ||
336 | |a nicht spezifiziert |b zzz |2 rdacontent | ||
337 | |a nicht spezifiziert |b z |2 rdamedia | ||
338 | |a nicht spezifiziert |b zu |2 rdacarrier | ||
520 | |a Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. | ||
520 | |a Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. | ||
650 | 7 | |a Particle size |2 Elsevier | |
650 | 7 | |a Luminescence lifetime |2 Elsevier | |
650 | 7 | |a Luminescence properties |2 Elsevier | |
650 | 7 | |a CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> |2 Elsevier | |
700 | 1 | |a Ma, Siming |4 oth | |
700 | 1 | |a Wang, Yu |4 oth | |
700 | 1 | |a Xu, Mai |4 oth | |
700 | 1 | |a Lu, Chengxi |4 oth | |
700 | 1 | |a Xiao, Linjiu |4 oth | |
700 | 1 | |a Deng, Shuguang |4 oth | |
773 | 0 | 8 | |i Enthalten in |n Elsevier Science |a Crowley, Martha ELSEVIER |t Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations |d 2018 |d an international journal on the physics and chemistry of optical materials and their applications, including devices |g Amsterdam [u.a.] |w (DE-627)ELV00185254X |
773 | 1 | 8 | |g volume:77 |g year:2018 |g pages:13-18 |g extent:6 |
856 | 4 | 0 | |u https://doi.org/10.1016/j.optmat.2018.01.015 |3 Volltext |
912 | |a GBV_USEFLAG_U | ||
912 | |a GBV_ELV | ||
912 | |a SYSFLAG_U | ||
936 | b | k | |a 70.00 |j Sozialwissenschaften allgemein: Allgemeines |q VZ |
936 | b | k | |a 71.00 |j Soziologie: Allgemeines |q VZ |
951 | |a AR | ||
952 | |d 77 |j 2018 |h 13-18 |g 6 |
author_variant |
y x yx |
---|---|
matchkey_str |
xieyingmasimingwangyuxumailuchengxixiaol:2018----:otoldyteiaduiecnerprisfaocifops4enecs |
hierarchy_sort_str |
2018transfer abstract |
bklnumber |
70.00 71.00 |
publishDate |
2018 |
allfields |
10.1016/j.optmat.2018.01.015 doi GBV00000000000669.pica (DE-627)ELV042142768 (ELSEVIER)S0925-3467(18)30015-6 DE-627 ger DE-627 rakwb eng 300 VZ 70.00 bkl 71.00 bkl Xie, Ying verfasserin aut Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals 2018transfer abstract 6 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> Elsevier Ma, Siming oth Wang, Yu oth Xu, Mai oth Lu, Chengxi oth Xiao, Linjiu oth Deng, Shuguang oth Enthalten in Elsevier Science Crowley, Martha ELSEVIER Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations 2018 an international journal on the physics and chemistry of optical materials and their applications, including devices Amsterdam [u.a.] (DE-627)ELV00185254X volume:77 year:2018 pages:13-18 extent:6 https://doi.org/10.1016/j.optmat.2018.01.015 Volltext GBV_USEFLAG_U GBV_ELV SYSFLAG_U 70.00 Sozialwissenschaften allgemein: Allgemeines VZ 71.00 Soziologie: Allgemeines VZ AR 77 2018 13-18 6 |
spelling |
10.1016/j.optmat.2018.01.015 doi GBV00000000000669.pica (DE-627)ELV042142768 (ELSEVIER)S0925-3467(18)30015-6 DE-627 ger DE-627 rakwb eng 300 VZ 70.00 bkl 71.00 bkl Xie, Ying verfasserin aut Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals 2018transfer abstract 6 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> Elsevier Ma, Siming oth Wang, Yu oth Xu, Mai oth Lu, Chengxi oth Xiao, Linjiu oth Deng, Shuguang oth Enthalten in Elsevier Science Crowley, Martha ELSEVIER Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations 2018 an international journal on the physics and chemistry of optical materials and their applications, including devices Amsterdam [u.a.] (DE-627)ELV00185254X volume:77 year:2018 pages:13-18 extent:6 https://doi.org/10.1016/j.optmat.2018.01.015 Volltext GBV_USEFLAG_U GBV_ELV SYSFLAG_U 70.00 Sozialwissenschaften allgemein: Allgemeines VZ 71.00 Soziologie: Allgemeines VZ AR 77 2018 13-18 6 |
allfields_unstemmed |
10.1016/j.optmat.2018.01.015 doi GBV00000000000669.pica (DE-627)ELV042142768 (ELSEVIER)S0925-3467(18)30015-6 DE-627 ger DE-627 rakwb eng 300 VZ 70.00 bkl 71.00 bkl Xie, Ying verfasserin aut Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals 2018transfer abstract 6 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> Elsevier Ma, Siming oth Wang, Yu oth Xu, Mai oth Lu, Chengxi oth Xiao, Linjiu oth Deng, Shuguang oth Enthalten in Elsevier Science Crowley, Martha ELSEVIER Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations 2018 an international journal on the physics and chemistry of optical materials and their applications, including devices Amsterdam [u.a.] (DE-627)ELV00185254X volume:77 year:2018 pages:13-18 extent:6 https://doi.org/10.1016/j.optmat.2018.01.015 Volltext GBV_USEFLAG_U GBV_ELV SYSFLAG_U 70.00 Sozialwissenschaften allgemein: Allgemeines VZ 71.00 Soziologie: Allgemeines VZ AR 77 2018 13-18 6 |
allfieldsGer |
10.1016/j.optmat.2018.01.015 doi GBV00000000000669.pica (DE-627)ELV042142768 (ELSEVIER)S0925-3467(18)30015-6 DE-627 ger DE-627 rakwb eng 300 VZ 70.00 bkl 71.00 bkl Xie, Ying verfasserin aut Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals 2018transfer abstract 6 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> Elsevier Ma, Siming oth Wang, Yu oth Xu, Mai oth Lu, Chengxi oth Xiao, Linjiu oth Deng, Shuguang oth Enthalten in Elsevier Science Crowley, Martha ELSEVIER Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations 2018 an international journal on the physics and chemistry of optical materials and their applications, including devices Amsterdam [u.a.] (DE-627)ELV00185254X volume:77 year:2018 pages:13-18 extent:6 https://doi.org/10.1016/j.optmat.2018.01.015 Volltext GBV_USEFLAG_U GBV_ELV SYSFLAG_U 70.00 Sozialwissenschaften allgemein: Allgemeines VZ 71.00 Soziologie: Allgemeines VZ AR 77 2018 13-18 6 |
allfieldsSound |
10.1016/j.optmat.2018.01.015 doi GBV00000000000669.pica (DE-627)ELV042142768 (ELSEVIER)S0925-3467(18)30015-6 DE-627 ger DE-627 rakwb eng 300 VZ 70.00 bkl 71.00 bkl Xie, Ying verfasserin aut Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals 2018transfer abstract 6 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> Elsevier Ma, Siming oth Wang, Yu oth Xu, Mai oth Lu, Chengxi oth Xiao, Linjiu oth Deng, Shuguang oth Enthalten in Elsevier Science Crowley, Martha ELSEVIER Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations 2018 an international journal on the physics and chemistry of optical materials and their applications, including devices Amsterdam [u.a.] (DE-627)ELV00185254X volume:77 year:2018 pages:13-18 extent:6 https://doi.org/10.1016/j.optmat.2018.01.015 Volltext GBV_USEFLAG_U GBV_ELV SYSFLAG_U 70.00 Sozialwissenschaften allgemein: Allgemeines VZ 71.00 Soziologie: Allgemeines VZ AR 77 2018 13-18 6 |
language |
English |
source |
Enthalten in Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations Amsterdam [u.a.] volume:77 year:2018 pages:13-18 extent:6 |
sourceStr |
Enthalten in Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations Amsterdam [u.a.] volume:77 year:2018 pages:13-18 extent:6 |
format_phy_str_mv |
Article |
bklname |
Sozialwissenschaften allgemein: Allgemeines Soziologie: Allgemeines |
institution |
findex.gbv.de |
topic_facet |
Particle size Luminescence lifetime Luminescence properties CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> |
dewey-raw |
300 |
isfreeaccess_bool |
false |
container_title |
Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations |
authorswithroles_txt_mv |
Xie, Ying @@aut@@ Ma, Siming @@oth@@ Wang, Yu @@oth@@ Xu, Mai @@oth@@ Lu, Chengxi @@oth@@ Xiao, Linjiu @@oth@@ Deng, Shuguang @@oth@@ |
publishDateDaySort_date |
2018-01-01T00:00:00Z |
hierarchy_top_id |
ELV00185254X |
dewey-sort |
3300 |
id |
ELV042142768 |
language_de |
englisch |
fullrecord |
<?xml version="1.0" encoding="UTF-8"?><collection xmlns="http://www.loc.gov/MARC21/slim"><record><leader>01000caa a22002652 4500</leader><controlfield tag="001">ELV042142768</controlfield><controlfield tag="003">DE-627</controlfield><controlfield tag="005">20230626000638.0</controlfield><controlfield tag="007">cr uuu---uuuuu</controlfield><controlfield tag="008">180726s2018 xx |||||o 00| ||eng c</controlfield><datafield tag="024" ind1="7" ind2=" "><subfield code="a">10.1016/j.optmat.2018.01.015</subfield><subfield code="2">doi</subfield></datafield><datafield tag="028" ind1="5" ind2="2"><subfield code="a">GBV00000000000669.pica</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(DE-627)ELV042142768</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(ELSEVIER)S0925-3467(18)30015-6</subfield></datafield><datafield tag="040" ind1=" " ind2=" "><subfield code="a">DE-627</subfield><subfield code="b">ger</subfield><subfield code="c">DE-627</subfield><subfield code="e">rakwb</subfield></datafield><datafield tag="041" ind1=" " ind2=" "><subfield code="a">eng</subfield></datafield><datafield tag="082" ind1="0" ind2="4"><subfield code="a">300</subfield><subfield code="q">VZ</subfield></datafield><datafield tag="084" ind1=" " ind2=" "><subfield code="a">70.00</subfield><subfield code="2">bkl</subfield></datafield><datafield tag="084" ind1=" " ind2=" "><subfield code="a">71.00</subfield><subfield code="2">bkl</subfield></datafield><datafield tag="100" ind1="1" ind2=" "><subfield code="a">Xie, Ying</subfield><subfield code="e">verfasserin</subfield><subfield code="4">aut</subfield></datafield><datafield tag="245" ind1="1" ind2="0"><subfield code="a">Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals</subfield></datafield><datafield tag="264" ind1=" " ind2="1"><subfield code="c">2018transfer abstract</subfield></datafield><datafield tag="300" ind1=" " ind2=" "><subfield code="a">6</subfield></datafield><datafield tag="336" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zzz</subfield><subfield code="2">rdacontent</subfield></datafield><datafield tag="337" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">z</subfield><subfield code="2">rdamedia</subfield></datafield><datafield tag="338" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zu</subfield><subfield code="2">rdacarrier</subfield></datafield><datafield tag="520" ind1=" " ind2=" "><subfield code="a">Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material.</subfield></datafield><datafield tag="520" ind1=" " ind2=" "><subfield code="a">Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material.</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">Particle size</subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">Luminescence lifetime</subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">Luminescence properties</subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup></subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Ma, Siming</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Wang, Yu</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Xu, Mai</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Lu, Chengxi</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Xiao, Linjiu</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Deng, Shuguang</subfield><subfield code="4">oth</subfield></datafield><datafield tag="773" ind1="0" ind2="8"><subfield code="i">Enthalten in</subfield><subfield code="n">Elsevier Science</subfield><subfield code="a">Crowley, Martha ELSEVIER</subfield><subfield code="t">Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations</subfield><subfield code="d">2018</subfield><subfield code="d">an international journal on the physics and chemistry of optical materials and their applications, including devices</subfield><subfield code="g">Amsterdam [u.a.]</subfield><subfield code="w">(DE-627)ELV00185254X</subfield></datafield><datafield tag="773" ind1="1" ind2="8"><subfield code="g">volume:77</subfield><subfield code="g">year:2018</subfield><subfield code="g">pages:13-18</subfield><subfield code="g">extent:6</subfield></datafield><datafield tag="856" ind1="4" ind2="0"><subfield code="u">https://doi.org/10.1016/j.optmat.2018.01.015</subfield><subfield code="3">Volltext</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_USEFLAG_U</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_ELV</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">SYSFLAG_U</subfield></datafield><datafield tag="936" ind1="b" ind2="k"><subfield code="a">70.00</subfield><subfield code="j">Sozialwissenschaften allgemein: Allgemeines</subfield><subfield code="q">VZ</subfield></datafield><datafield tag="936" ind1="b" ind2="k"><subfield code="a">71.00</subfield><subfield code="j">Soziologie: Allgemeines</subfield><subfield code="q">VZ</subfield></datafield><datafield tag="951" ind1=" " ind2=" "><subfield code="a">AR</subfield></datafield><datafield tag="952" ind1=" " ind2=" "><subfield code="d">77</subfield><subfield code="j">2018</subfield><subfield code="h">13-18</subfield><subfield code="g">6</subfield></datafield></record></collection>
|
author |
Xie, Ying |
spellingShingle |
Xie, Ying ddc 300 bkl 70.00 bkl 71.00 Elsevier Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals |
authorStr |
Xie, Ying |
ppnlink_with_tag_str_mv |
@@773@@(DE-627)ELV00185254X |
format |
electronic Article |
dewey-ones |
300 - Social sciences |
delete_txt_mv |
keep |
author_role |
aut |
collection |
elsevier |
remote_str |
true |
illustrated |
Not Illustrated |
topic_title |
300 VZ 70.00 bkl 71.00 bkl Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> Elsevier |
topic |
ddc 300 bkl 70.00 bkl 71.00 Elsevier Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> |
topic_unstemmed |
ddc 300 bkl 70.00 bkl 71.00 Elsevier Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> |
topic_browse |
ddc 300 bkl 70.00 bkl 71.00 Elsevier Particle size Elsevier Luminescence lifetime Elsevier Luminescence properties Elsevier CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> |
format_facet |
Elektronische Aufsätze Aufsätze Elektronische Ressource |
format_main_str_mv |
Text Zeitschrift/Artikel |
carriertype_str_mv |
zu |
author2_variant |
s m sm y w yw m x mx c l cl l x lx s d sd |
hierarchy_parent_title |
Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations |
hierarchy_parent_id |
ELV00185254X |
dewey-tens |
300 - Social sciences, sociology & anthropology |
hierarchy_top_title |
Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations |
isfreeaccess_txt |
false |
familylinks_str_mv |
(DE-627)ELV00185254X |
title |
Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals |
ctrlnum |
(DE-627)ELV042142768 (ELSEVIER)S0925-3467(18)30015-6 |
title_full |
Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals |
author_sort |
Xie, Ying |
journal |
Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations |
journalStr |
Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations |
lang_code |
eng |
isOA_bool |
false |
dewey-hundreds |
300 - Social sciences |
recordtype |
marc |
publishDateSort |
2018 |
contenttype_str_mv |
zzz |
container_start_page |
13 |
author_browse |
Xie, Ying |
container_volume |
77 |
physical |
6 |
class |
300 VZ 70.00 bkl 71.00 bkl |
format_se |
Elektronische Aufsätze |
author-letter |
Xie, Ying |
doi_str_mv |
10.1016/j.optmat.2018.01.015 |
dewey-full |
300 |
title_sort |
controlled synthesis and luminescence properties of camoo<ce:inf loc="post">4</ce:inf>:eu<ce:sup loc="post">3+</ce:sup> microcrystals |
title_auth |
Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals |
abstract |
Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. |
abstractGer |
Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. |
abstract_unstemmed |
Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material. |
collection_details |
GBV_USEFLAG_U GBV_ELV SYSFLAG_U |
title_short |
Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals |
url |
https://doi.org/10.1016/j.optmat.2018.01.015 |
remote_bool |
true |
author2 |
Ma, Siming Wang, Yu Xu, Mai Lu, Chengxi Xiao, Linjiu Deng, Shuguang |
author2Str |
Ma, Siming Wang, Yu Xu, Mai Lu, Chengxi Xiao, Linjiu Deng, Shuguang |
ppnlink |
ELV00185254X |
mediatype_str_mv |
z |
isOA_txt |
false |
hochschulschrift_bool |
false |
author2_role |
oth oth oth oth oth oth |
doi_str |
10.1016/j.optmat.2018.01.015 |
up_date |
2024-07-06T22:01:20.826Z |
_version_ |
1803868732996452352 |
fullrecord_marcxml |
<?xml version="1.0" encoding="UTF-8"?><collection xmlns="http://www.loc.gov/MARC21/slim"><record><leader>01000caa a22002652 4500</leader><controlfield tag="001">ELV042142768</controlfield><controlfield tag="003">DE-627</controlfield><controlfield tag="005">20230626000638.0</controlfield><controlfield tag="007">cr uuu---uuuuu</controlfield><controlfield tag="008">180726s2018 xx |||||o 00| ||eng c</controlfield><datafield tag="024" ind1="7" ind2=" "><subfield code="a">10.1016/j.optmat.2018.01.015</subfield><subfield code="2">doi</subfield></datafield><datafield tag="028" ind1="5" ind2="2"><subfield code="a">GBV00000000000669.pica</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(DE-627)ELV042142768</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(ELSEVIER)S0925-3467(18)30015-6</subfield></datafield><datafield tag="040" ind1=" " ind2=" "><subfield code="a">DE-627</subfield><subfield code="b">ger</subfield><subfield code="c">DE-627</subfield><subfield code="e">rakwb</subfield></datafield><datafield tag="041" ind1=" " ind2=" "><subfield code="a">eng</subfield></datafield><datafield tag="082" ind1="0" ind2="4"><subfield code="a">300</subfield><subfield code="q">VZ</subfield></datafield><datafield tag="084" ind1=" " ind2=" "><subfield code="a">70.00</subfield><subfield code="2">bkl</subfield></datafield><datafield tag="084" ind1=" " ind2=" "><subfield code="a">71.00</subfield><subfield code="2">bkl</subfield></datafield><datafield tag="100" ind1="1" ind2=" "><subfield code="a">Xie, Ying</subfield><subfield code="e">verfasserin</subfield><subfield code="4">aut</subfield></datafield><datafield tag="245" ind1="1" ind2="0"><subfield code="a">Controlled synthesis and luminescence properties of CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup> microcrystals</subfield></datafield><datafield tag="264" ind1=" " ind2="1"><subfield code="c">2018transfer abstract</subfield></datafield><datafield tag="300" ind1=" " ind2=" "><subfield code="a">6</subfield></datafield><datafield tag="336" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zzz</subfield><subfield code="2">rdacontent</subfield></datafield><datafield tag="337" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">z</subfield><subfield code="2">rdamedia</subfield></datafield><datafield tag="338" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zu</subfield><subfield code="2">rdacarrier</subfield></datafield><datafield tag="520" ind1=" " ind2=" "><subfield code="a">Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material.</subfield></datafield><datafield tag="520" ind1=" " ind2=" "><subfield code="a">Pure tetragonal-phased Ca0.9MoO4:0.1Eu3+ (CaMoO4:Eu3+) microcrystals with varying particle sizes were prepared via a co-deposition in water/oil (w/o) phase method. The particle sizes of as-prepared samples were controlled by calcination temperature and calcination time, and the crystallinity of the samples enhances with increasing particle size. The luminescence properties of CaMoO4:Eu3+ microcrystals were studied with varying particle size. The results reveal that the intensity of emission spectra of the CaMoO4:Eu3+ samples increases with increasing particle size, and they have closely correlation with each other. It is the same with the luminescence lifetime. The luminescence lifetime of the CaMoO4:Eu3+ samples decreases from 0.637 ms to 0.447 ms with increasing particle size from 0.12 μm to 1.79 μm, respectively. This study not only provides information for size-dependent luminescence properties of CaMoO4:Eu3+ but also gives a reference for potential applications in high voltage electric porcelain material.</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">Particle size</subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">Luminescence lifetime</subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">Luminescence properties</subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="650" ind1=" " ind2="7"><subfield code="a">CaMoO<ce:inf loc="post">4</ce:inf>:Eu<ce:sup loc="post">3+</ce:sup></subfield><subfield code="2">Elsevier</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Ma, Siming</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Wang, Yu</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Xu, Mai</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Lu, Chengxi</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Xiao, Linjiu</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Deng, Shuguang</subfield><subfield code="4">oth</subfield></datafield><datafield tag="773" ind1="0" ind2="8"><subfield code="i">Enthalten in</subfield><subfield code="n">Elsevier Science</subfield><subfield code="a">Crowley, Martha ELSEVIER</subfield><subfield code="t">Strangers in their hometown: Demographic change, revitalization and community engagement in new Latino destinations</subfield><subfield code="d">2018</subfield><subfield code="d">an international journal on the physics and chemistry of optical materials and their applications, including devices</subfield><subfield code="g">Amsterdam [u.a.]</subfield><subfield code="w">(DE-627)ELV00185254X</subfield></datafield><datafield tag="773" ind1="1" ind2="8"><subfield code="g">volume:77</subfield><subfield code="g">year:2018</subfield><subfield code="g">pages:13-18</subfield><subfield code="g">extent:6</subfield></datafield><datafield tag="856" ind1="4" ind2="0"><subfield code="u">https://doi.org/10.1016/j.optmat.2018.01.015</subfield><subfield code="3">Volltext</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_USEFLAG_U</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_ELV</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">SYSFLAG_U</subfield></datafield><datafield tag="936" ind1="b" ind2="k"><subfield code="a">70.00</subfield><subfield code="j">Sozialwissenschaften allgemein: Allgemeines</subfield><subfield code="q">VZ</subfield></datafield><datafield tag="936" ind1="b" ind2="k"><subfield code="a">71.00</subfield><subfield code="j">Soziologie: Allgemeines</subfield><subfield code="q">VZ</subfield></datafield><datafield tag="951" ind1=" " ind2=" "><subfield code="a">AR</subfield></datafield><datafield tag="952" ind1=" " ind2=" "><subfield code="d">77</subfield><subfield code="j">2018</subfield><subfield code="h">13-18</subfield><subfield code="g">6</subfield></datafield></record></collection>
|
score |
7.400505 |