Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation
Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process i...
Ausführliche Beschreibung
Autor*in: |
---|
Format: |
E-Artikel |
---|---|
Sprache: |
Englisch |
Erschienen: |
1989 |
---|
Reproduktion: |
Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 |
---|---|
Übergeordnetes Werk: |
in: Journal of Magnetism and Magnetic Materials - Amsterdam : Elsevier, 81(1989), 1-2, Seite 147-150 |
Übergeordnetes Werk: |
volume:81 ; year:1989 ; number:1-2 ; pages:147-150 |
Links: |
---|
Katalog-ID: |
NLEJ177678348 |
---|
LEADER | 01000caa a22002652 4500 | ||
---|---|---|---|
001 | NLEJ177678348 | ||
003 | DE-627 | ||
005 | 20210706055242.0 | ||
007 | cr uuu---uuuuu | ||
008 | 070505s1989 xx |||||o 00| ||eng c | ||
035 | |a (DE-627)NLEJ177678348 | ||
035 | |a (DE-599)GBVNLZ177678348 | ||
040 | |a DE-627 |b ger |c DE-627 |e rakwb | ||
041 | |a eng | ||
245 | 1 | 0 | |a Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation |
264 | 1 | |c 1989 | |
336 | |a nicht spezifiziert |b zzz |2 rdacontent | ||
337 | |a nicht spezifiziert |b z |2 rdamedia | ||
338 | |a nicht spezifiziert |b zu |2 rdacarrier | ||
520 | |a Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. | ||
533 | |f Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 | ||
700 | 1 | |a Raj, P. |4 oth | |
700 | 1 | |a Sathyamoorthy, A. |4 oth | |
700 | 1 | |a Krishnan, R. |4 oth | |
700 | 1 | |a Laridjani, M. |4 oth | |
773 | 0 | 8 | |i in |t Journal of Magnetism and Magnetic Materials |d Amsterdam : Elsevier |g 81(1989), 1-2, Seite 147-150 |w (DE-627)NLEJ177226366 |w (DE-600)1479000-2 |x 0304-8853 |7 nnns |
773 | 1 | 8 | |g volume:81 |g year:1989 |g number:1-2 |g pages:147-150 |
856 | 4 | 0 | |u http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4 |
912 | |a GBV_USEFLAG_H | ||
912 | |a ZDB-1-SDJ | ||
912 | |a GBV_NL_ARTICLE | ||
951 | |a AR | ||
952 | |d 81 |j 1989 |e 1-2 |h 147-150 |
matchkey_str |
article:03048853:1989----::mrhusutrdr0e0olufc |
---|---|
hierarchy_sort_str |
1989 |
publishDate |
1989 |
allfields |
(DE-627)NLEJ177678348 (DE-599)GBVNLZ177678348 DE-627 ger DE-627 rakwb eng Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation 1989 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 Raj, P. oth Sathyamoorthy, A. oth Krishnan, R. oth Laridjani, M. oth in Journal of Magnetism and Magnetic Materials Amsterdam : Elsevier 81(1989), 1-2, Seite 147-150 (DE-627)NLEJ177226366 (DE-600)1479000-2 0304-8853 nnns volume:81 year:1989 number:1-2 pages:147-150 http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4 GBV_USEFLAG_H ZDB-1-SDJ GBV_NL_ARTICLE AR 81 1989 1-2 147-150 |
spelling |
(DE-627)NLEJ177678348 (DE-599)GBVNLZ177678348 DE-627 ger DE-627 rakwb eng Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation 1989 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 Raj, P. oth Sathyamoorthy, A. oth Krishnan, R. oth Laridjani, M. oth in Journal of Magnetism and Magnetic Materials Amsterdam : Elsevier 81(1989), 1-2, Seite 147-150 (DE-627)NLEJ177226366 (DE-600)1479000-2 0304-8853 nnns volume:81 year:1989 number:1-2 pages:147-150 http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4 GBV_USEFLAG_H ZDB-1-SDJ GBV_NL_ARTICLE AR 81 1989 1-2 147-150 |
allfields_unstemmed |
(DE-627)NLEJ177678348 (DE-599)GBVNLZ177678348 DE-627 ger DE-627 rakwb eng Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation 1989 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 Raj, P. oth Sathyamoorthy, A. oth Krishnan, R. oth Laridjani, M. oth in Journal of Magnetism and Magnetic Materials Amsterdam : Elsevier 81(1989), 1-2, Seite 147-150 (DE-627)NLEJ177226366 (DE-600)1479000-2 0304-8853 nnns volume:81 year:1989 number:1-2 pages:147-150 http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4 GBV_USEFLAG_H ZDB-1-SDJ GBV_NL_ARTICLE AR 81 1989 1-2 147-150 |
allfieldsGer |
(DE-627)NLEJ177678348 (DE-599)GBVNLZ177678348 DE-627 ger DE-627 rakwb eng Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation 1989 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 Raj, P. oth Sathyamoorthy, A. oth Krishnan, R. oth Laridjani, M. oth in Journal of Magnetism and Magnetic Materials Amsterdam : Elsevier 81(1989), 1-2, Seite 147-150 (DE-627)NLEJ177226366 (DE-600)1479000-2 0304-8853 nnns volume:81 year:1989 number:1-2 pages:147-150 http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4 GBV_USEFLAG_H ZDB-1-SDJ GBV_NL_ARTICLE AR 81 1989 1-2 147-150 |
allfieldsSound |
(DE-627)NLEJ177678348 (DE-599)GBVNLZ177678348 DE-627 ger DE-627 rakwb eng Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation 1989 nicht spezifiziert zzz rdacontent nicht spezifiziert z rdamedia nicht spezifiziert zu rdacarrier Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 Raj, P. oth Sathyamoorthy, A. oth Krishnan, R. oth Laridjani, M. oth in Journal of Magnetism and Magnetic Materials Amsterdam : Elsevier 81(1989), 1-2, Seite 147-150 (DE-627)NLEJ177226366 (DE-600)1479000-2 0304-8853 nnns volume:81 year:1989 number:1-2 pages:147-150 http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4 GBV_USEFLAG_H ZDB-1-SDJ GBV_NL_ARTICLE AR 81 1989 1-2 147-150 |
language |
English |
source |
in Journal of Magnetism and Magnetic Materials 81(1989), 1-2, Seite 147-150 volume:81 year:1989 number:1-2 pages:147-150 |
sourceStr |
in Journal of Magnetism and Magnetic Materials 81(1989), 1-2, Seite 147-150 volume:81 year:1989 number:1-2 pages:147-150 |
format_phy_str_mv |
Article |
institution |
findex.gbv.de |
isfreeaccess_bool |
false |
container_title |
Journal of Magnetism and Magnetic Materials |
authorswithroles_txt_mv |
Raj, P. @@oth@@ Sathyamoorthy, A. @@oth@@ Krishnan, R. @@oth@@ Laridjani, M. @@oth@@ |
publishDateDaySort_date |
1989-01-01T00:00:00Z |
hierarchy_top_id |
NLEJ177226366 |
id |
NLEJ177678348 |
language_de |
englisch |
fullrecord |
<?xml version="1.0" encoding="UTF-8"?><collection xmlns="http://www.loc.gov/MARC21/slim"><record><leader>01000caa a22002652 4500</leader><controlfield tag="001">NLEJ177678348</controlfield><controlfield tag="003">DE-627</controlfield><controlfield tag="005">20210706055242.0</controlfield><controlfield tag="007">cr uuu---uuuuu</controlfield><controlfield tag="008">070505s1989 xx |||||o 00| ||eng c</controlfield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(DE-627)NLEJ177678348</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(DE-599)GBVNLZ177678348</subfield></datafield><datafield tag="040" ind1=" " ind2=" "><subfield code="a">DE-627</subfield><subfield code="b">ger</subfield><subfield code="c">DE-627</subfield><subfield code="e">rakwb</subfield></datafield><datafield tag="041" ind1=" " ind2=" "><subfield code="a">eng</subfield></datafield><datafield tag="245" ind1="1" ind2="0"><subfield code="a">Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation</subfield></datafield><datafield tag="264" ind1=" " ind2="1"><subfield code="c">1989</subfield></datafield><datafield tag="336" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zzz</subfield><subfield code="2">rdacontent</subfield></datafield><datafield tag="337" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">z</subfield><subfield code="2">rdamedia</subfield></datafield><datafield tag="338" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zu</subfield><subfield code="2">rdacarrier</subfield></datafield><datafield tag="520" ind1=" " ind2=" "><subfield code="a">Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics.</subfield></datafield><datafield tag="533" ind1=" " ind2=" "><subfield code="f">Elsevier Journal Backfiles on ScienceDirect 1907 - 2002</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Raj, P.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Sathyamoorthy, A.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Krishnan, R.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Laridjani, M.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="773" ind1="0" ind2="8"><subfield code="i">in</subfield><subfield code="t">Journal of Magnetism and Magnetic Materials</subfield><subfield code="d">Amsterdam : Elsevier</subfield><subfield code="g">81(1989), 1-2, Seite 147-150</subfield><subfield code="w">(DE-627)NLEJ177226366</subfield><subfield code="w">(DE-600)1479000-2</subfield><subfield code="x">0304-8853</subfield><subfield code="7">nnns</subfield></datafield><datafield tag="773" ind1="1" ind2="8"><subfield code="g">volume:81</subfield><subfield code="g">year:1989</subfield><subfield code="g">number:1-2</subfield><subfield code="g">pages:147-150</subfield></datafield><datafield tag="856" ind1="4" ind2="0"><subfield code="u">http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_USEFLAG_H</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">ZDB-1-SDJ</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_NL_ARTICLE</subfield></datafield><datafield tag="951" ind1=" " ind2=" "><subfield code="a">AR</subfield></datafield><datafield tag="952" ind1=" " ind2=" "><subfield code="d">81</subfield><subfield code="j">1989</subfield><subfield code="e">1-2</subfield><subfield code="h">147-150</subfield></datafield></record></collection>
|
series2 |
Elsevier Journal Backfiles on ScienceDirect 1907 - 2002 |
ppnlink_with_tag_str_mv |
@@773@@(DE-627)NLEJ177226366 |
format |
electronic Article |
delete_txt_mv |
keep |
collection |
NL |
remote_str |
true |
illustrated |
Not Illustrated |
issn |
0304-8853 |
topic_title |
Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation |
format_facet |
Elektronische Aufsätze Aufsätze Elektronische Ressource |
format_main_str_mv |
Text Zeitschrift/Artikel |
carriertype_str_mv |
zu |
author2_variant |
p r pr a s as r k rk m l ml |
hierarchy_parent_title |
Journal of Magnetism and Magnetic Materials |
hierarchy_parent_id |
NLEJ177226366 |
hierarchy_top_title |
Journal of Magnetism and Magnetic Materials |
isfreeaccess_txt |
false |
familylinks_str_mv |
(DE-627)NLEJ177226366 (DE-600)1479000-2 |
title |
Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation |
spellingShingle |
Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation |
ctrlnum |
(DE-627)NLEJ177678348 (DE-599)GBVNLZ177678348 |
title_full |
Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation |
journal |
Journal of Magnetism and Magnetic Materials |
journalStr |
Journal of Magnetism and Magnetic Materials |
lang_code |
eng |
isOA_bool |
false |
recordtype |
marc |
publishDateSort |
1989 |
contenttype_str_mv |
zzz |
container_start_page |
147 |
container_volume |
81 |
format_se |
Elektronische Aufsätze |
title_sort |
amorphous sputtered zr"1"0fe"9"0 foil: surface degradation |
title_auth |
Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation |
abstract |
Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. |
abstractGer |
Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. |
abstract_unstemmed |
Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics. |
collection_details |
GBV_USEFLAG_H ZDB-1-SDJ GBV_NL_ARTICLE |
container_issue |
1-2 |
title_short |
Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation |
url |
http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4 |
remote_bool |
true |
author2 |
Raj, P. Sathyamoorthy, A. Krishnan, R. Laridjani, M. |
author2Str |
Raj, P. Sathyamoorthy, A. Krishnan, R. Laridjani, M. |
ppnlink |
NLEJ177226366 |
mediatype_str_mv |
z |
isOA_txt |
false |
hochschulschrift_bool |
false |
author2_role |
oth oth oth oth |
up_date |
2024-07-06T09:45:51.334Z |
_version_ |
1803822459870248960 |
fullrecord_marcxml |
<?xml version="1.0" encoding="UTF-8"?><collection xmlns="http://www.loc.gov/MARC21/slim"><record><leader>01000caa a22002652 4500</leader><controlfield tag="001">NLEJ177678348</controlfield><controlfield tag="003">DE-627</controlfield><controlfield tag="005">20210706055242.0</controlfield><controlfield tag="007">cr uuu---uuuuu</controlfield><controlfield tag="008">070505s1989 xx |||||o 00| ||eng c</controlfield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(DE-627)NLEJ177678348</subfield></datafield><datafield tag="035" ind1=" " ind2=" "><subfield code="a">(DE-599)GBVNLZ177678348</subfield></datafield><datafield tag="040" ind1=" " ind2=" "><subfield code="a">DE-627</subfield><subfield code="b">ger</subfield><subfield code="c">DE-627</subfield><subfield code="e">rakwb</subfield></datafield><datafield tag="041" ind1=" " ind2=" "><subfield code="a">eng</subfield></datafield><datafield tag="245" ind1="1" ind2="0"><subfield code="a">Amorphous sputtered Zr"1"0Fe"9"0 foil: Surface degradation</subfield></datafield><datafield tag="264" ind1=" " ind2="1"><subfield code="c">1989</subfield></datafield><datafield tag="336" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zzz</subfield><subfield code="2">rdacontent</subfield></datafield><datafield tag="337" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">z</subfield><subfield code="2">rdamedia</subfield></datafield><datafield tag="338" ind1=" " ind2=" "><subfield code="a">nicht spezifiziert</subfield><subfield code="b">zu</subfield><subfield code="2">rdacarrier</subfield></datafield><datafield tag="520" ind1=" " ind2=" "><subfield code="a">Conversion electron Mossbauer spectroscopic and X-ray diffraction studies on sputtered amorphous foils of Zr"1"0Fe"9"0 are carried out over a period of several months. One side of the foils is found to undergo degradation and the texture of the α-Fe layer formed in this process is found to be distinctly different from that reported for melt-spun ribbon samples. This is ascribed to the rather high tendency of this system to undergo composition segregation. The fabrication parameters therefore become crucial in determining the ferromagnetic Curie temperature and the overall short and medium range order in the bulk as well as the surface degradation characteristics.</subfield></datafield><datafield tag="533" ind1=" " ind2=" "><subfield code="f">Elsevier Journal Backfiles on ScienceDirect 1907 - 2002</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Raj, P.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Sathyamoorthy, A.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Krishnan, R.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="700" ind1="1" ind2=" "><subfield code="a">Laridjani, M.</subfield><subfield code="4">oth</subfield></datafield><datafield tag="773" ind1="0" ind2="8"><subfield code="i">in</subfield><subfield code="t">Journal of Magnetism and Magnetic Materials</subfield><subfield code="d">Amsterdam : Elsevier</subfield><subfield code="g">81(1989), 1-2, Seite 147-150</subfield><subfield code="w">(DE-627)NLEJ177226366</subfield><subfield code="w">(DE-600)1479000-2</subfield><subfield code="x">0304-8853</subfield><subfield code="7">nnns</subfield></datafield><datafield tag="773" ind1="1" ind2="8"><subfield code="g">volume:81</subfield><subfield code="g">year:1989</subfield><subfield code="g">number:1-2</subfield><subfield code="g">pages:147-150</subfield></datafield><datafield tag="856" ind1="4" ind2="0"><subfield code="u">http://linkinghub.elsevier.com/retrieve/pii/0304-8853(89)90242-4</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_USEFLAG_H</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">ZDB-1-SDJ</subfield></datafield><datafield tag="912" ind1=" " ind2=" "><subfield code="a">GBV_NL_ARTICLE</subfield></datafield><datafield tag="951" ind1=" " ind2=" "><subfield code="a">AR</subfield></datafield><datafield tag="952" ind1=" " ind2=" "><subfield code="d">81</subfield><subfield code="j">1989</subfield><subfield code="e">1-2</subfield><subfield code="h">147-150</subfield></datafield></record></collection>
|
score |
7.3994465 |